Note. Thermoplastics (except «Noryl»).
Wash the part in soapy water and then in clean water.
Clean the area to be repaired with a lint-free cloth soaked in antistatic solvent.
Wipe the surface with a clean, dry, lint-free cloth.
Remove the crack with a P 150 nozzle at a width of 50 mm.
Blow out the element with compressed air and clean the area to be repaired with a lint-free cloth soaked in antistatic solvent.
Wipe the surface with a clean, dry, lint-free cloth.
Preheat the soldering iron.
Cut the stainless steel gear to match the shape of the support.
Spot weld with a soldering iron tip on the ends to secure the mounting bracket.
Allow each weld point to cool for 2 seconds using a cooler.
Install the stainless steel engagement and hold it with the appropriate tool.
Cover the stainless steel frame with plastic material.
Allow the repair area to cool for two seconds using a cooler.
Polish the surface first with P 80-P 150, then with P 240.
Blow out the element with compressed air and clean the area to be repaired with a lint-free cloth soaked in antistatic solvent.
Define the Part Shape (drilled a hole), to give it its original look.
Apply paint if necessary.